MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow 3-6371 UV GEL
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Former Dow Corning product.

Information provided by Dow Corning

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/cc
@Temperature 25.0 °C
Viscosity 910 cPdynamic
 
Mechanical PropertiesOriginal ValueComments
Penetration P(0), 1/10 mm >= 140
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.90e+12 ohm-cm
Dielectric Constant 2.81
@Frequency 100 Hz
 2.81
@Frequency 100000 Hz
Dielectric Strength 300 V/mil
Dissipation Factor <= 0.00010
@Frequency 100000 Hz
 0.0050
@Frequency 100 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -80.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Appearancetranslucent
Coloramber
Flowableyes
Gel Hardness (Grams/Penetration)40
Self Levelingyes
Water Resistantyes
Working Time (min)10080

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 3-4170 DIELECTRIC GEL KIT
Master Bond UV15SP-1 Low Viscosity, UV Curable System
Chosun Refractories SCX-70 I Special SiC Castable
Chosun Refractories AMC-70 Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2

PDOWCO334 / 106035

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.