MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hytrel® HTR8241 TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 65 Shore D High Performance Polyester Elastomer Developed for Extrusion

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Melt Density 1.07 g/cc
@Temperature 240 °C
0.0387 lb/in³
@Temperature 464 °F
Water Absorption 0.70 %
@Thickness 2.00 mm
0.70 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
0.200 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.017 cm/cm0.017 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.016 cm/cm0.016 in/inISO 294-4, 2577
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 606015s; ISO 48-4
 <= 63<= 63ISO 48-4
Tensile Stress at Strain  12.5 MPa
@Strain 5.0 %
1810 psi
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 18.0 MPa
@Strain 10 %
2610 psi
@Strain 10 %
ISO 527-1/-2
 21.0 MPa
@Strain 50 %
3050 psi
@Strain 50 %
ISO 527-1/-2
Tensile Modulus 0.360 GPa52.2 ksiISO 527-1/-2
Flexural Modulus 0.360 GPa52.2 ksiISO 178
Poissons Ratio 0.480.48
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -40.0 °C
4.76 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 1.40 J/cm²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
Tear Strength 200 kN/m1140 plinormal; ISO 34-1
 210 kN/m1200 pliparallel; ISO 34-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.00e+12 ohm-cm7.00e+12 ohm-cmIEC 62631-3-1
Surface Resistance 2.00e+14 ohm2.00e+14 ohmIEC 62631-3-2
Dielectric Strength 18.0 kV/mm457 kV/inIEC 60243-1
Dissipation Factor  0.011
@Frequency 1e+6 Hz
0.011
@Frequency 1e+6 Hz
IEC 62631-2-1
 0.011
@Frequency 100 Hz
0.011
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 200 µm/m-°C111 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 200 µm/m-°C111 µin/in-°FISO 11359-1/-2
Specific Heat Capacity 2.07 J/g-°C
@Temperature 240 °C
0.495 BTU/lb-°F
@Temperature 464 °F
Melt
Thermal Conductivity 0.150 W/m-K
@Temperature 240 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 464 °F
Melt
Melting Point 211 °C412 °F10°C/min; ISO 11357-1/-3
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 225 - 240 °C437 - 464 °FRange, Extrusion
 235 °C455 °FOptimum, Extrusion
 240 °C464 °FOptimum, Injection
 230 - 250 °C446 - 482 °FRange, Injection
Mold Temperature 45.0 °C113 °FOptimum, Injection
 40.0 - 50.0 °C104 - 122 °FInjection
Drying Temperature 110 °C230 °FInjection
 100 - 120 °C212 - 248 °FExtrusion
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourExtrusion, Dehumidified Dryer
 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.060 %<= 0.060 %Extrusion
 <= 0.080 %<= 0.080 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)5.44E-08
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hytrel® 8238 TPC-ET
Celanese Hytrel® HTR8163HVBK TPC-ET
Celanese Hytrel® HTR8341C BK320 TPC-ET
Celanese Hytrel® HTR8068 TPC-ET-FR(17)
Celanese Hytrel® HTR8223 BK320 TPC-ET

PDSX5212 / 197852

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.