MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Weld Epoxy Adhesive EC-2216 B/A in chemical composition. Scotch-Weld epoxy adhesive 2216 B/A may be used for aircraft and aerospace applications if proper Certificates of Test have been issued an issued and material meets all aircraft manufacturer’s specification requirements.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 5000 - 9000 cPAccelerator, RVF #7 spindle, 20 rpm
 11000 - 15000 cPBase, RVF #7 spindle, 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 35 - 50
Shear Modulus 49.6 ksi
@Temperature 24.0 °C
Torsion Pendulum Method
 218.8 ksi
@Temperature 0.000 °C
Torsion Pendulum Method
 282.3 ksi
@Temperature -40.0 °C
Torsion Pendulum Method
 318.85 ksi
@Temperature -60.0 °C
Torsion Pendulum Method
 398 ksi
@Temperature -100 °C
Torsion Pendulum Method
Shear Strength 1260 psiOverlap, Etched Al, Salt Spray at RT for 30 days
 1390 psiOverlap, Etched Al, 100% RH at 49°C for 30 days
 1950 psiOverlap, Etched Al, Tap water at RT for 30 days
 2500 psiOverlap, Etched Al, Anti-icing Fluid at RT for 7 days
 2500 psiOverlap, Etched Al, Hydraulic Oil at RT for 30 days
 2500 psiOverlap, Etched Al, JP-4 for 30 days
 3000 psiOverlap, Etched Al, Hydrocarbon Fluid for 7 days
 3500 psiOverlap, Etched Al, Air at 149°C for 40 days
 140 psi
@Temperature 82.0 °C
Overlap, Etched Aluminum; ASTM D1002
 1700 psi
@Temperature 24.0 °C
Overlap, Etched Aluminum; ASTM D1002
 3000 psi
@Temperature -53.0 °C
Overlap, Etched Aluminum; ASTM D1002
Peel Strength 25.0 pli
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+12 ohm-cm@ 500 volts DC
Dielectric Constant 14.17
@Frequency 1000 Hz
Dielectric Strength 630 kV/in
Dissipation Factor 0.229
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 81.0 µm/m-°C
@Temperature -50.0 - 0.000 °C
 207 µm/m-°C
@Temperature 60.0 - 150 °C
Thermal Conductivity 1.37 BTU-in/hr-ft²-°F
 
Processing PropertiesOriginal ValueComments
Cure Time 12.0 - 16.0 hourTime to Handling Strength
 
Descriptive Properties
AppearanceAmberAccelerator
 TranslucentBase
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive
3M Scotch-Weld™ 2216 B/A Gray Two-Part Epoxy Adhesive 2216 B/A Gray
3M Scotch-Weld™ 2216 B/A Tan Non-Sag Two-Part Epoxy Adhesive 2216 B/A Tan Non-Sag
3M Scotch-Weld™ DP-100 Clear Adhesive in Duo-Pak Cartridges

PMM34637 / 169384

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.