MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TEGOMER® H-Si 6440P Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product description: TEGOMER® H-Si 6440 P is a polyester modified siloxane which is delivered in pellet form with excellent compatibility in thermoplastic and duroplastic resins.

Application: TEGOMER® H-Si 6440 P is used as additive to improve the scratch resistance of engineering resins, TPEs and polyolefins. TEGOMER® H-Si 6440 P lowers the COF of materials such as TPE-Vs. TEGOMER® H-Si 6440 P is used for PA/GF and PP/GF based compounds. TEGOMER® H-Si 6440 P is used as compatible internal lubricant and release agent, e.g. mold release of SEBS based air bag covers. The additive is well suited to improve bulk and surface characteristics of final parts, especially notched impacts strength in filled polyolefins. TEGOMER® H-Si 6440 P can be used as additive for:

  • polyolefins
  • polyamides
  • polyesters/ polycarbonates
  • thermoplastic elastomers
  • thermosets
Benefits: TEGOMER® H-Si 6440 P used as an additive for polymer formulation. It improves the processing by:
  • better mould fill release behavior
  • good internal lubrication
  • improved rheology of polymer melt
The surface properties are improved by:
  • enhanced scratch and wear resistance
  • lower surface frictions
  • higher surface gloss
  • better glass fiber wetting/ lower fiber brakes
It improves bulk properties by:
  • higher impact strength
  • higher tensile strength
  • reduction of brittleness
  • hydrophobizing

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 54.0 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.10 %
 
Descriptive Properties
Appearancepellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Molding Compound
Evonik TEGOMER® P 122 Dispersing additive
Evonik TEGOMER® M-Si 2650 Additive
Evonik TEGOMER® H-Si 2311 Additive
Evonik TEGOMER® DA 100 N Dispersant

PEVONIL586 / 196790

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.