MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik TEGOMER® DA 100 N Dispersant
Categories: Other Engineering Material

Material Notes: Product description: TEGOMER® DA 100 N is a polymeric dispersant technology which can be applied for the dispersion of solid particles in hydrophobic media.

Application:

  • TEGOMER® DA 100 N is used as dispersant in liquid pastes for the dispersion and stabilization of organic pigments and fillers.
  • TEGOMER® DA 100 N can be applied in mineral and vegetable oil for the dispersion of solid particles coming from the filler and pigment range, nanoparticles or also solid additive ingredients, e.g. antioxidants, flame retardants and others. Those pastes or colorants are used for polyolefines or styrenic thermoplastic systems.
  • TEGOMER® DA 100 N is a suitable dispersant for the manufacture of pigment dispersion in phthalates and adipates which are intended to be used for PVC application.
  • TEGOMER® DA 100 N has a good compatibility in 100 % systems based on acrylates, hydrophobic polyether polyols or polyester polyols whereas hydrophilic polyether polyols are not compatible with it.
Benefits: TEGOMER® DA 100 N is a liquid dispersant applicable in a wide range of hydrophobic phases. It allows the manufacture of thermoplastic and duroplastic materials with efficient color strength development due to high pigment stability and dispersion degree. Pastes based on TEGOMER® DA 100 N are long term stable since this polymeric dispersant allows even in low viscous media to avoid settlement. TEGOMER® DA 100 N allows higher loading of pigments and nanomaterials in hydrophobic media.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³
Viscosity 4000 - 7000 cP4000 - 7000 cP
 
Descriptive Properties
Appearanceamber liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Struktol TR 255 Processing Additive, Dispersant
Struktol TR EBS Processing Additive, Dispersant
Evonik TEGOMER® DA 640 Dispersant
Struktol TR 251 Processing Additive, Dispersant
Dow Latex XZ 92229.03 Experimental Latex

PEVONIL577 / 196781

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.