Product description: Grilon F 40 NL natural 6018 is a nucleated and lubricated high viscosity polyamide 6. This product exhibits the following features:- Good gas barrier
- Good mechanical properties
- Good barrier against oils and fats
- Good optical properties
Application examples: Grilon F 40 NL natural 6018 is suitable for the production of mono and co-extruded blown and cast films. Barrier layer in multi-layer films for food packaging, mostly used as vacuum bags (meat, fish, cheese) and thermoformed pouches or sausage casings.Information provided by EMS Grivory. |