MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilon® F 40 NL PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Product description: Grilon F 40 NL natural 6018 is a nucleated and lubricated high viscosity polyamide 6. This product exhibits the following features:
  • Good gas barrier
  • Good mechanical properties
  • Good barrier against oils and fats
  • Good optical properties
Application examples: Grilon F 40 NL natural 6018 is suitable for the production of mono and co-extruded blown and cast films. Barrier layer in multi-layer films for food packaging, mostly used as vacuum bags (meat, fish, cheese) and thermoformed pouches or sausage casings.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³Dry; ISO 1183
Water Absorption 9.0 %9.0 %Sim. to ISO 62
Moisture Absorption 3.00 %3.00 %Sim. to ISO 62
Water Vapor Transmission 15.0 g/m²/day0.966 g/100 in²/day23°C/85% RH; ISO 15106-1/-2
Melt Flow 25 g/10 min25 g/10 mincm³/10min Volumetric; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 35.0 MPa5080 psiISO 527-3
Film Tensile Strength at Yield, TD 30.0 MPa4350 psiISO 527-3
Film Elongation at Break, MD 700 %700 %ISO 527-3
Film Elongation at Break, TD 700 %700 %ISO 527-3
Film Elongation at Yield, MD 15 %15 %ISO 527-3
Film Elongation at Yield, TD 15 %15 %ISO 527-3
Tensile Modulus 0.750 GPa109 ksiConditioned; ISO 527-1/-2
 3.00 GPa435 ksiDry; ISO 527-1/-2
Coefficient of Friction, Dynamic 0.250.25ISO 8295
Tear Strength 30.0 kN/m171 pliTrouser Tear Resistance, Parallel; ISO 6383-1
 30.0 kN/m171 pliTrouser Tear Resistance, Normal; ISO 6383-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °F10°C/min; ISO 11357-1/-3
 
Optical PropertiesMetricEnglishComments
Gloss 100 %100 %60°; ISO 2813
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood contact
 
Descriptive Properties
Carbon Dioxide Transmission Rate, cm³/(m²*d*bar)250ISO 15105-1/-2; 23°C/ 85% RH
 80ISO 15105-1/-2; 23°C/0% RH
Elmendorf Tear Resistance, Normal (N)10ISO 6383-2
Elmendorf Tear Resistance, Parallel (N)10ISO 6383-2
Food contactEU Requirements
FormGranules
Gelboflextest [holes/m²], EMS800
Oxygen Transmission Rate, cm³/(m²*d*bar)25ISO 15105-1/-2; 23°C/0% RH
 50ISO 15105-1/-2; 23°C/ 85% RH
PackagingNon oriented film
 Oriented film
 Paper coating
 Tubes
ProcessingBlown Film Extrusion
 Film Extrusion
 Other Extrusion
Product AttributesBarrier Properties
 High viscosity
 Nucleated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax PF531 Polypropylene Homopolymer, Radiation Resistant
Radici Radilon® S 40FL (dry) Nylon 6
Nylacast Aquanyl Nylon 612 Copolymer
LyondellBasell Pro-fax PF511 Polypropylene Homopolymer, Radiation Resistant
LyondellBasell Montell 1900 UHMW Polyethylene

PGRH238 / 156947

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.