MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond LED405Med One component, nanosilica filled LED curable system
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Meets ISO 10993-5 for cytotoxicity
  • Fast cure with appropriate LED light
  • Resists sterilization
  • Not oxygen inhibited
  • Can cure up to 1/8 inch thick
  • Outstanding optical clarity
Master Bond LED405Med is a one part system that cures upon exposure to a 405 nm LED light without requiring a UV light source. It will cure without any oxygen inhibition. Its most special feature is that its main constituent is a nanofilled resin. This results in lower shrinkage upon curing and greater dimensional stability. By using LED light and not UV, it is intrinsically less hazardous and more user friendly. Master Bond LED405Med requires no mixing and cures rapidly upon exposure to 405 nm LED light. The speed of cure depends upon the intensity of the light source, the thickness of the layer, and the distance of the light source from the material being cured. Realistically, the light intensity should be 1-4 watts/cm2. Master Bond strongly advises end users to consult with their LED light provider in order to choose the best light source. LED405Med will typically cure in 30-45 seconds in thinner sections, while thicker sections will take longer to cure. LED405Med bonds well to a wide variety of substrates including metals, plastics and glass. It is a superior electrical insulator and is resistant to water, several acids and bases, oils and fuels. LED405Med resists many sterilization methods such as gamma, EtO and radiation. It has a particular affinity for acrylics, polycarbonates, and glass.

Product Advantages:

  • One component system needs no mixing
  • Cures by LED light, UV light not required
  • Nanofilled system
  • Unsurpassed low shrinkage upon curing
  • Reasonably good physical strength properties
  • Superb dimensional stability

Information provided by Masterbond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/cc
Viscosity 2000 - 8000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65 - 75
Tensile Strength 3000 - 4000 psi
Tensile Modulus 150000 - 200000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 4.2
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 65.0 - 70.0 µm/m-°C
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -60.0 °F
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.50
 
Processing PropertiesOriginal ValueComments
Shelf Life 3.00 - 6.00 MonthIn original unopened containers, with no exposure to light
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cookson Group Plaskon® SMT-B-2FPI Molding Compound for PBGA and CSP
Master Bond LED401 White One Component LED Curable Adhesive System
Cookson Group Plaskon® PPF-165 Conventional Epoxy Molding Compound
Raschig Group EN 5007 Epoxy Molding Compound
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled

PMASTM725 / 233782

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.