MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Oxford Polymers 30GF-25PTFE 30% Glass Fiber/PTFE Reinforced Polyphenylene Sulfide  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled

Material Notes: 30% Glass Fiber/PTFE Reinforced Polyphenylene Sulfide

Information provided by Oxford Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.66 g/ccASTM D792
Filler Content 30 %
Water Absorption 0.020 %ASTM D570
Linear Mold Shrinkage 0.0020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 19000 psiASTM D638
Elongation at Break 1.5 %ASTM D638
Flexural Strength 27.0 ksiASTM D790
Flexural Modulus 1600 ksiASTM D790
Izod Impact, Notched 1.40 ft-lb/in
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 500 °FASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC Fluon® RB1020S 20% Glass Fiber, PTFE Filled Compound
AGC Fluon® RB1015S 15% Glass Fiber, PTFE Filled Compound
RTP Company RTP 1303 TFE 15 LE  Polyphenylene Sulfide (PPS) Glass Fiber 20% - PTFE 15% - Low Extractable
RTP Company RTP 1303 TFE 10 Polyphenylene Sulfide (PPS), Glass Fiber Reinforced - PTFE Lubricated
Rogers Corporation RO3003 Ceramic-Filled PTFE Composite, High Frequency Circuit Material

POX23 / 55872

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.