MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials Silopren™ LSR 3486/20 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding process allows for complex part geometry and exact dimensions. LSR elastomers are generally suitable for short cycle time injection and full automatic flash-less processing. Color pastes are available to pigmenting addition cure productions of LSR's.

All LSR grades are platinum cured materials which are mixed in a 1:1 ratio by weight.

Industries and Applications: The Momentive portfolio of products is used for a wide variety of applications in the Automotive, Aviation and Aerospace, Consumer Goods, Consumer Electronics, Healthcare and Energy Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/cc
Linear Mold Shrinkage 0.027 cm/cmvulcanized 10 sec at 200°C; Without post-cure
 0.035 cm/cmvulcanized 10 sec at 200°C then post-cured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 22
Tensile Strength 8.00 MPa
Elongation at Break 1000 %
Tear Strength 10.0 kN/mDie B
Compression Set 25 %Non post-cured
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 20 %translucent; thickness unknown
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 20.0 °Ccool nozzle and cylinder to prevent premature vulcanization
Mold Temperature 140 - 230 °Cshort vulcanization time required (a few seconds)
Injection Pressure 5.00 - 15.0 MPadepends on feed channel
Hold Pressure 5.00 MPa
 
Descriptive Properties
AppearanceTranslucent

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 3-4170 DIELECTRIC GEL KIT
Dow C6-530 LIQUID SILICONE RUBBER KIT
Elkem (Bluestar Silicones) CAF® 1 Extra Fluid Silicone Rubber
Elkem (Bluestar Silicones) CAF® 7037 Silicone Rubber
Wacker Lumisil® LR 7601/80 Liquid Silicone Rubber

PGE8V763 / 109023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.