MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Universal Wire Works HP9-4-20 (AMS 6468) Low Alloy Steel Welding Wire
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Material Notes: Alloy HP9-4-20 is a premium quality low alloy steel filler metal for use with the gas tungsten arc and gas metal arc welding processes. Alloy HP9-4-20 is designed to weld those low-alloy steels having compositions similar to that of this wire and requiring a combination of high strength and high notch toughness without the need for post-weld heat treatment.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.16 %0.16 %
Chromium, Cr 1.0 %1.0 %
Cobalt, Co 3.75 %3.75 %
Copper, Cu <= 0.10 %<= 0.10 %
Hydrogen, H <= 0.0010 %<= 0.0010 %
Iron, Fe >= 83.7 %>= 83.7 %As Remainder
Manganese, Mn 0.50 %0.50 %
Molybdenum, Mo 0.45 %0.45 %
Nickel, Ni 10 %10 %
Nitrogen, N <= 0.0080 %<= 0.0080 %
Oxygen, O <= 0.0050 %<= 0.0050 %
Phosphorus, P <= 0.0080 %<= 0.0080 %
Silicon, Si 0.20 %0.20 %
Sulfur, S <= 0.0080 %<= 0.0080 %
Vanadium, V 0.080 %0.080 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A514 Steel, grade D, plate thickness ≤ 19 mm
Bethlehem Steel ASTM A514 Grade P >2-1/2 to 4 in. thick, steel plate
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties
SCM420 Carburizing Bearing Steel (Composition Spec)
ThyssenKrupp COR-TEN A Structural Steel

NUWW352 / 19762

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.