MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt STYPOL® 040-4917 Acrylic Modified Gel Coat
Categories: Polymer; Thermoset

Material Notes: STYPOL® 040-4917 is a clear, acrylic modified NPG® isophthalic gel coat. STYPOL® 040-4917 has been designed for use in the manufacture of cultured marble, onyx, and granite.

Features and Benefits:

  • Excellent dimensional stability during hot and cold water cycling
  • Excellent chemical and water resistance
  • Good sprayability
  • Excellent nonsagging properties
  • High clarity
  • UV Light stabilized
  • Good color retention
  • Suitable for low pressure spray equipment
  • Meets gel coat test specifications according to ANSI Z124.3
  • Meets the BAAQMD, Regulation 8-50-1, Method 26 (Bay Area AQMD of Northern California)

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Volatile Organic Compounds (VOC) Content 49.5 g/l49.5 g/l
Brookfield Viscosity 2800 cP2800 cPRVF #3 Spindle @ 20 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 3535Model #934; ASTM D2583
Tensile Strength 71.7 MPa10400 psiASTM D638
Elongation at Break 2.9 %2.9 %ASTM D638
Tensile Modulus 3.03 GPa440 ksiASTM D638
Flexural Strength 128 MPa18500 psiASTM D790
Flexural Modulus 3.93 GPa570 ksiASTM D790
Impact Test 4.65 J3.43 ft-lbASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Cure Time 45.0 min0.750 hourCastable Time refers to the point at which a gel coat film is ready to be cast upon
Gel Time 12.0 min12.0 min100 g mass, 2.0% Arkema Luperox ® DDM-9
 
Descriptive Properties
Thixotropic Index7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Medalist® MD-135 Thermoplastic Elastomer
Gabriel Versamid® G 490 Amidoamine Resin

PPOLYN9268 / 231863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.