MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gabriel Versamid® G 490 Amidoamine Resin
Categories: Polymer; Thermoset

Material Notes: Versamid® products have proven to be superior coatings resins in many applications, such as industrial maintenance and marine coatings, high-performance architectural paints and high-solids and conventional coatings.

Advantages:

  • Highly resistant to chemical and water corrosion
  • Strong adhesion to a variety of substrates
  • Long pot life
  • Lower sensitivity to substrate impurities
  • Most comply with FDA regulations
Principal Applications: High-solids coatings and castings

Comments/Advantages: Extremely low-viscosity, long pot life

Information provided by Gabriel Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.947 g/cc0.0342 lb/in³
Solids Content 100 %100 %Theo
Viscosity 100 - 400 cP100 - 400 cP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 46.9 MPa6800 psiAfter 7 days 25°C cure
Elongation at Break 4.6 %4.6 %After 7 days 25°C cure
Flexural Strength 141 MPa20400 psiAfter 7 days 25°C cure
Flexural Modulus 4.50 GPa653 ksiAfter 7 days 25°C cure
Compressive Strength 51.7 MPa7500 psiAfter 7 days 25°C cure
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg <= 80.0 °C<= 176 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 9.0<= 9.0
 
Processing PropertiesMetricEnglishComments
Cure Time 840 min14.0 hourTack Free Time; 3 wet mils
 >= 1440 min>= 24.0 hourThrough Cure; 3 wet mils
Pot Life 480 min480 min60% solids
Gel Time 235 min235 min200 mg Mass
 
Descriptive Properties
Amine Value370-400[mg KOH/g]
Chemical Resistance to 10% Acetic Acid5.45% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to 10% H4SO41% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to 10% HCl0.65% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to 10% NAOH0.48% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to Ethanol7.74% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to MEKDES% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to Xylene23.52% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical TypeAmidoamine
PHR for Max DSC, Tg50190 EEW Epoxy
Theo Amine Hydrogen Equl Wt.95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polynt STYPOL® 040-4917 Acrylic Modified Gel Coat

PGABR987 / 230688

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.