MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco AREMCOLOX™ 502-1400 (Full-Fired) Dense Alumina  (discontinued **)
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Parts fabricated to print. Excellent physical properties and corrosion resistance. For pump liners, nozzles, guides. Standard crucibles and bolts, nuts and washers from 4-40 to 1/4-20.

Vendors: Aremco offers a range of machinable ceramics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.90 g/cc
Porosity 0.00 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 9.0
Flexural Strength 46000 psi
Compressive Strength 340000 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 9.3
@Frequency 1e+6 Hz
Dielectric Strength 225 V/mil
Dissipation Factor 0.0018
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.50 µin/in-°F
@Temperature 20.0 °C
Thermal Conductivity 220 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 3000 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco AREMCOLOX™ 502-400 Machinable Glass Ceramic
Aremco AREMCOLOX™ 502-1100 (Unfired) Machinable Alumino-Silicate
Aremco AREMCOLOX™ 502-1100 (Full-Fired) Dense Alumino-Silicate
Borosilicate Glass
Borosilicate Glass, Low Expansion

ZCAREM06 / 547

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.