MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Label-Lyte™ 50TD200 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A clear, transverse-direction shrinkable, one-side treated, polyolefin film. With a density below 1.0, this film facilitates floatation and supports the PET bottle-to-bottle recycling process (where available). This film is designed for use as a monoweb in shrink sleeve labeling of contoured containers, such as contoured plastic and glass bottles, aluminum and steel beverage cans, beaded metals cans and aerosol containers. The treated clear layer is for printing and is intended to be reverse-printed. 50TD200 Sleeve is suitable for all heat shrink processes and sealable with common solvent )THF.

Availability: Europe and North America

Key Features:

  • Outstanding and consistent traverse-direction shrinkage, in applications requiring up to 50% shrink
  • Density <1.0 before and after shrinkage, which facilitates separation of label from bottle to support bottle-to bottle recycling (where available)
  • Excellent gloss and ink adhesion
  • Consistent machinablility in all heat sleeve shrink processes
  • Sealable with common solvent (THF)
Applications:
  • Beverage, Alcoholic
  • Beverage, Carbonated
  • Beverage, Mineral Waters
  • Dairy Products
  • Dry Foods and Beverage Powders
  • Food, bottled and canistered
  • Health and Beauty Care
  • Household and Detergents
Uses:
  • Heat Shrink Sleeve Labels
Processing Method: Heat Reactive Adhesive, Offset Ebeam Printing, Solvent Flexographic Printing, Solvent Rotogravure Printing, UV Flexographic Printing and UV Offset Lithography Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccExxonMobil Method
Thickness 2.00 milExxonMobil Method
Coating Weight 28.0 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction 0.37Untreated Surface; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 4.0 %
@Temperature 80.0 °C
Free Shrinkage; ASTM D2732
 9.0 %
@Temperature 100 °C
Free Shrinkage; ASTM D2732
Shrinkage, TD 33 %
@Temperature 80.0 °C
Free Shrinkage; ASTM D2732
 66 %
@Temperature 100 °C
Free Shrinkage; ASTM D2732
 
Optical PropertiesOriginal ValueComments
Haze 9.0 %ExxonMobil Method
Gloss 83 %45°; ExxonMobil Method
 
Descriptive Properties
Treatment50 dyne/cmPrint Surface
Yield15500 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® SEG7 35% Glass Filled PA6 (Dry)
Eastman CB12 PET
Eastman BD445 PET
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 75 Gauge
DAK Americas Laser+® MB912 PET

PEX99556 / 175792

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.