MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Eastman CB12 PET  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good overall bottle properties. This polymer is formulated to provide improved efficiencies in preform and bottle production while delivering a robust processing window. Bottles made with CB12 deliver improved barrier with continued excellent performance in creep and environmental stress-crack resistance.
The pellets have a weight of 2.0g/100pellets

Applications/Uses

  • Bottles
  • Carbonated soft drink containers
  • Key Attributes

  • Excellent performance in stress-crack resistance
  • Fast, efficient processing
  • Improved barrier
  • Robust processing window
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Bulk Density 0.810 g/cc0.0293 lb/in³Poured (Mexico Produced); ASTM D1895
     0.845 g/cc0.0305 lb/in³Poured (US Produced); ASTM D1895
     0.880 g/cc0.0318 lb/in³Vibrated (Mexico Produced); ASTM D1895
     0.898 g/cc0.0324 lb/in³Vibrated (US Produced); ASTM D1895
    Density 1.40 g/cc0.0506 lb/in³Crystalline Density; ASTM D1505
    Melt Density 1.20 g/cc
    @Temperature 285 °C
    0.0434 lb/in³
    @Temperature 545 °F
    ASTM D1238
    Particle Size 2500 µm2500 µmPellet Size
    Viscosity Measurement 0.80 - 0.840.80 - 0.84Intrinsic; EMN-A-AC-G-V-1
     
    Thermal PropertiesMetricEnglishComments
    Heat of Fusion 59.0 J/g25.4 BTU/lbASTM E793
    Specific Heat Capacity 1.20 J/g-°C0.287 BTU/lb-°FASTM E1269
     1.40 J/g-°C
    @Temperature 80.0 °C
    0.335 BTU/lb-°F
    @Temperature 176 °F
    ASTM E1269
     1.50 J/g-°C
    @Temperature 100 °C
    0.359 BTU/lb-°F
    @Temperature 212 °F
    ASTM E1269
     1.90 J/g-°C
    @Temperature 200 °C
    0.454 BTU/lb-°F
    @Temperature 392 °F
    ASTM E1269
     2.10 J/g-°C
    @Temperature 280 °C
    0.502 BTU/lb-°F
    @Temperature 536 °F
    ASTM E1269
    Melting Point 245 °C473 °FCrystalline Peak; ASTM D3418
     
    Descriptive Properties
    Acetaldehyde<3ppmTEPO-A-AN-G-GC-67
    Color, CIE a*-3.0 to 0.0VGAS-A-AN-G-RS-001
    Color, CIE b*-1.8 to 1.0VGAS-A-AN-G-RS-001
    Color, CIE L*76.5 minVGAS-A-AN-G-RS-001
    Fines, wt%, max0.05VGAS-A-AN-G-GA-1
    Pellet ShapeCubical

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    DAK Americas Laser+® MB912 PET
    Iran Petrochemical (PCC) PET BG-845 Polyethylene Terephthalate
    SABIC BC 110 Crystalline Polyethylene Terephthalate
    Eastman BD445 PET
    SABIC BC 112 Crystalline Polyethylene Terephthalate

    PE9144 / 35201

    Specialty Compounds RTP Company

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.