MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Wacker Wacker® Finish CT 45 E Silicone Softener Emulsion
Categories: Fluid; Polymer

Material Notes: Product description: WACKER® FINISH CT 45 E is a nonionic macro emulsion of a reactive, aminofunctional silicone fluid.

Application: WACKER® FINISH CT 45 E is particularly suitable as softener for the impregnation of fibers and textiles. WACKER® FINISH CT 45 E imparts a very soft, drapable, and elastic touch to woven and knitted fabrics. WACKER® FINISH CT 45 E is considered to be the best softening agent for PES/cotton fabrics. WACKER® FINISH CT 45 E improves the wash-and - wear properties and the crease recovery angle, sewability and tear strength and reduces abrasion loss. The effects are fast to washing and dry cleaning. WACKER® FINISH CT 45 E has very little effect on the degree of whiteness when usual application conditions are adhered to. Generally, no adverse effect on the shade or color fastness properties of coloured goods is observed. As part of formulations used as fill fibre finish WACKER® FINISH CT 45 E imparts excellent slickness and resilience to the fibre.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 40 %40 %
pH 5.05.0
 
Descriptive Properties
Appearancemilky-white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Belsil® ADM 1370 Amino-Functional Silicone
Wacker Belsil® ADM 6102 E Amino-Functional Silicone
Wacker Belsil® ADM 6057 E Amodimethicone (Macro-emulsion)
Wacker Belsil® ADM 1650 Amodimethicone
Wacker Wacker® Finish CT 34 E Silicone Softener Emulsion

PWACK9770 / 205299

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.