Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength properties, along with excellent drawability of these resins, make them versatile packaging film resins. Availability: Latin America, North America and South America Additive: - Antiblock: No
- Slip: No
- Processing Aid: No
- Thermal Stabilizer: Yes
Applications: - Cast Film
- Cast Stretch Film
- Packaging Films
Information provided by ExxonMobil Chemical |