MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil LL 3001.32 Cast Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior strength properties, along with excellent drawability, make this a very versatile packaging film resin.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: No
  • Thermal Stabilizer: Yes
Applications:
  • Freezer Film
  • Heavy Duty Bags
  • Ice Bags
  • Trash Bags
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ExxonMobil Method
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 8.41 MPa1220 psiASTM D882
Film Tensile Strength at Yield, TD 7.72 MPa1120 psiASTM D882
Film Elongation at Break, MD 340 %340 %ASTM D882
Film Elongation at Break, TD 790 %790 %ASTM D882
Puncture Energy 3.28 J2.42 ft-lbExxonMobil
Elmendorf Tear Strength, MD 11.8 g/micron300 g/milASTM D1922
Elmendorf Tear Strength, TD 29.53 g/micron750.0 g/milASTM D1922
Dart Drop 3.15 g/micron80.0 g/milASTM D1709
Film Tensile Strength at Break, MD 66.1 MPa9590 psiASTM D882
Film Tensile Strength at Break, TD 38.2 MPa5540 psiASTM D882
1% Secant Modulus, MD 119 MPa17300 psiASTM D882
1% Secant Modulus, TD 145 MPa21000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 124 °C255 °FPeak Melting Temperature; ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 2.2 %2.2 %ASTM D1003
Gloss 89 %89 %45°; ASTM D2457
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos R01C-01 Polypropylene Random Copolymer
Ineos N02G-00 Polypropylene Impact Copolymer
ExxonMobil VISTANEX™ L-140
ExxonMobil VISTANEX™ L-100
ExxonMobil PP7684KN Impact Copolymer

PEXB214 / 37519

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.