MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Adhesive 2214 Hi-Temp is an aluminum filled, deaerated products fro use where higher strengths are required between 82-177°C. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a paste consistency epoxy adhesive designed for bonding metals and many high temperature plastics such as fiberglass reinforced plastic, polyester, and phenolics

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 15 - 30 cP15 - 30 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 88>= 88
Tensile Strength, Ultimate 55.2 MPa8000 psi
Elongation at Break 1.0 %1.0 %
Modulus of Elasticity 5.52 GPa800 ksi
Shear Strength  6.21 MPa
@Temperature 177 °C
900 psi
@Temperature 351 °F
Aluminum Overlap
 13.8 MPa
@Temperature -53.0 °C
2000 psi
@Temperature -63.4 °F
Aluminum Overlap
 13.8 MPa
@Temperature 24.0 °C
2000 psi
@Temperature 75.2 °F
Aluminum Overlap
 17.2 MPa
@Temperature 121 °C
2500 psi
@Temperature 250 °F
Aluminum Overlap
 17.2 MPa
@Temperature 149 °C
2500 psi
@Temperature 300 °F
Aluminum Overlap
 20.7 MPa
@Temperature 82.0 °C
3000 psi
@Temperature 180 °F
Aluminum Overlap
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 9.40e+13 ohm-cm9.40e+13 ohm-cm
Surface Resistance 1.10e+17 ohm1.10e+17 ohm
Dielectric Constant  6.2
@Temperature 23.0 °C
6.2
@Temperature 73.4 °F
ASTM D150
 7.6
@Temperature 60.0 °C
7.6
@Temperature 140 °F
ASTM D150
 7.8
@Temperature 90.0 °C
7.8
@Temperature 194 °F
ASTM D150
 8.0
@Temperature 104 °C
8.0
@Temperature 219 °F
ASTM D150
Dielectric Strength 13.7 kV/mm
@Thickness 0.965 mm
347 kV/in
@Thickness 0.0380 in
Dissipation Factor  0.021
@Temperature 23.0 °C
0.021
@Temperature 73.4 °F
 0.023
@Temperature 60.0 °C
0.023
@Temperature 140 °F
 0.025
@Temperature 90.0 °C
0.025
@Temperature 194 °F
 0.025
@Temperature 104 °C
0.025
@Temperature 219 °F
Arc Resistance 119 sec119 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 48.0 µm/m-°C
@Temperature 0.000 - 80.0 °C
26.7 µin/in-°F
@Temperature 32.0 - 176 °F
Thermal Conductivity 0.327 W/m-K2.27 BTU-in/hr-ft²-°F
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp New Formula Epoxy Adhesive

PMM34632 / 169379

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.