MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a paste consistency epoxy adhesive designed for bonding metals and many high temperature plastics such as fiberglass reinforced plastic, polyester, and phenolics

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 50 - 200 cP50 - 200 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 85>= 85
Tensile Strength, Ultimate 62.1 MPa9000 psi
Elongation at Break <= 2.0 %<= 2.0 %
Modulus of Elasticity 4.83 GPa700 ksi
Shear Strength  2.07 MPa
@Temperature -53.0 °C
300 psi
@Temperature -63.4 °F
Aluminum Overlap
 2.76 MPa
@Temperature 177 °C
400 psi
@Temperature 351 °F
Aluminum Overlap
 4.14 MPa
@Temperature 149 °C
600 psi
@Temperature 300 °F
Aluminum Overlap
 10.3 MPa
@Temperature 121 °C
1500 psi
@Temperature 250 °F
Aluminum Overlap
 27.6 MPa
@Temperature 24.0 °C
4000 psi
@Temperature 75.2 °F
Aluminum Overlap
 31.0 MPa
@Temperature 82.0 °C
4500 psi
@Temperature 180 °F
Aluminum Overlap
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.50e+13 ohm-cm2.50e+13 ohm-cm
Dielectric Strength 22.4 kV/mm
@Thickness 0.991 mm
570 kV/in
@Thickness 0.0390 in
Arc Resistance 26 sec26 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 130 µm/m-°C
@Temperature -30.0 - 100 °C
72.2 µin/in-°F
@Temperature -22.0 - 212 °F
Thermal Conductivity 0.209 W/m-K1.45 BTU-in/hr-ft²-°F
 
Descriptive Properties
AppearanceCream

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp New Formula Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive

PMM34634 / 169381

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.