MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 823 RTM Epoxy - 6K-5HS-HTA-370 Composite
Categories: Polymer; Thermoset; Epoxy

Material Notes: CYCOM® 823 RTM is a liquid epoxy resin system. It is primarily available as a one-part system, with one working week out-life at room temperature so as to remove the requirement for customers to carry out resin mixing and its associated quality control processes. Its frozen storage shelf-life is 6 months at 0°F (-18°C). If extended ambient storage is required then the resin could be supplies as a two-part system. CYCOM 823 RTM’s viscosity is low enough at room temperature to allow injection without having to heat either the resin or the transfer pipework. When the resin is heated to the cure temperature its viscosity is further reduced, helping to ensure full wet-out of the reinforcing fibers. CYCOM 823 RTM is fully cured after one hour at 255°F (125°C) giving a continuous dry service performance of 230°F (110°C) and a continuous hot/wet service performance of 195°F (90°C). CYCOM 823 RTM neat resin has high elongation, high GIC and high KIC values, all of which are indicative of a tough material. CYCOM 823 RTM is compatible with the usual range of reinforcing fibers utilized for the manufacture of composite components, i.e., carbon, glass, aramid, etc. For reinforcement preforming operations a fully compatible binder system, CYCOM® 790 RTM has been developed for use with CYCOM 823 RTM. The binder is available pre-coated onto fabrics of the customers’ choice. A separate datasheet for CYCOM 790 is available on request.

Features & Benefits:

  • Available as a one- or two-part system
  • 4 – 5 day out-life at room temperature, indefinite as a two-part system
  • Six-month shelf-life at 0°F (-18°C)
  • Room temperature injectable
  • 250 cps initial injection viscosity
  • <20 cps minimum viscosity
  • One hour at 255°F (125°C) cure
  • 230°F (110°C) continuous dry service performance
  • 195°F (90°C) continuous hot/wet service performance
  • High neat resin toughness
  • Fully compatible toughness enhancing binder, CYCOM 790 RTM, available
Mechanical property data for composite of 823 RTM epoxy with 52% fiber volume 6K-5HS-HTA-370 in warp orientation.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccNeat Resin
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 160000 psiAmbient
 130000 psi
@Temperature 70.0 °C
Wet
Flexural Modulus 71.7 GPaAmbient
 69.7 GPa
@Temperature 70.0 °C
Wet
Compressive Strength 778 MPaAmbient
 560 MPa
@Temperature 70.0 °C
Wet
Compressive Modulus 59200 MPaAmbient
 60000 MPa
@Temperature 70.0 °C
Wet
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °Cwet
 110 °Cdry
Glass Transition Temp, Tg 108 °CE' onset, 40 hr water boil, Neat Resin
 121 °Cpeak tan delta, wet, 40 hr water boil, Neat Resin
 125 °CE' onset, Neat Resin
 135 °Cpeak tan delta, Neat Resin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexFlow® RTM 6 180°C Epoxy System for Resin Transfer Molding Monocomponent System
RTP Company RTP 2200 AR 35  Polyetheretherketone (PEEK) Aramid Fiber 35%
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Goodfellow Carbon/Polyetheretherketone (PEEK) Composite
Goodfellow Carbon/Epoxy Composite Sheet

PCYTED086a / 233606

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.