MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Plastcom SLOVAMID® 6 GF 30 AS PA6 reinforced with glass fiber, anti-static agent  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: PA 6 for injection molding, reinforced with 30% glass fiber, contains antistatic agent for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, gears, covers of electric tools, automobile mirror housings, cooling screws of blowers, electromotors, bearing parts in the automotive industry. Delivered in natural mode and in the full RAL color scale.

Information Provided by Plastcom spol. s r.o.

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³STN EN ISO 1183-1
Filler Content 30 %30 %
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inSTN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inSTN EN ISO 294-4
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 175 MPa25400 psiSTN EN ISO 527-2
Elongation at Break 3.0 %3.0 %STN EN ISO 527-2
Tensile Modulus 9.80 GPa1420 ksiSTN EN ISO 527-2
Flexural Strength 220 MPa31900 psiSTN EN ISO 178
Flexural Modulus 8.60 GPa1250 ksiSTN EN ISO 178
Charpy Impact Unnotched  6.00 J/cm²
@Temperature -20.0 °C
28.6 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched  0.800 J/cm²
@Temperature -20.0 °C
3.81 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmSTN 34 6460
Surface Resistance 1.00e+12 ohm1.00e+12 ohmSTN 34 6460
Dielectric Strength 35.0 kV/mm889 kV/inSTN EN 60243-2
Comparative Tracking Index 350 V350 VSTN EN 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FSTN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FSTN EN ISO 75-2 (A)
Vicat Softening Point 250 °C482 °FSTN EN ISO 306
Flammability, UL94 HBHB
Glow Wire Flammability Index 650 °C
@Thickness 3.00 mm
1200 °F
@Thickness 0.118 in
STN EN 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 270 °C464 - 518 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
Moisture Content 0.15 %0.15 %STN EN ISO 3344
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Pebax® MV 1074 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® MH 1657 Polyether Block Amide (PEBA)
Sanyo J-STAT 3180 Antistatic Additive
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive
Murtfeldt Muralen® Black Antistatic Polyethylene, Conductive

PPLACO530 / 140931

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.