MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Du-Co Ceramics S-461 Magnesia
Categories: Ceramic; Oxide; Magnesium Oxide

Material Notes: Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are custom designed to meet specifications for purity and crushability.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.38 g/cc
Porosity >= 14 %
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 2000 - 10000 psi
Compressive Strength 2000 - 15000 psi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.7 µm/m-°C
@Temperature 25.0 - 700 °C
Maximum Service Temperature, Air >= 2000 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 <= 0.15 %
CaO <= 0.35 %
Fe2O3 <= 0.15 %
MgO >= 99.4 %
SiO2 <= 0.15 %
 
Descriptive Properties
B+Cd (ppm)<= 30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec Sikor® S Cordierite
Du-Co Ceramics S-464 Magnesia
MarkeTech Magnesium Oxide (MgO) Single Crystal Substrate
Mateck MgO
Morgan Advanced Ceramics Luminex™ 993 Magnesia

CDUC11 / 108434

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.