MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Luminex™ 993 Magnesia
Categories: Ceramic; Oxide; Magnesium Oxide

Material Notes: Porous electrofused material offering consistent electrical performance at elevated temperatures. Tailorable properties.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 - 2.70 g/cc0.0795 - 0.0975 lb/in³Fired, tailorable
Porosity 24 - 39 %24 - 39 %Apparent, fully dense, tailorable
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 7.00 - 85.0 MPa1020 - 12300 psi3-point, tailorable
Compressive Strength 12.0 - 190 MPa1740 - 27600 psitailorable
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+9 - 1.20e+11 ohm-cm
@Temperature 600 °C
1.00e+9 - 1.20e+11 ohm-cm
@Temperature 1110 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.7 - 14.3 µm/m-°C
@Temperature 200 - 500 °C
6.50 - 7.94 µin/in-°F
@Temperature 392 - 932 °F
 13.0 - 14.8 µm/m-°C
@Temperature 20.0 - 1000 °C
7.22 - 8.22 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity  8.00 - 32.0 W/m-K
@Temperature 20.0 °C
55.5 - 222 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 8.00 - 32.0 W/m-K
@Temperature 400 °C
55.5 - 222 BTU-in/hr-ft²-°F
@Temperature 752 °F
Maximum Service Temperature, Air 800 - 1200 °C1470 - 2190 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MarkeTech Magnesium Oxide (MgO) Single Crystal Substrate
MarkeTech Repton 914 Magnesia MgO
MarkeTech Repton EXP 22 Magnesia MgO
Mateck MgO
CeramTec Sikor® S Cordierite

CMORG37 / 90415

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.