Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 33% Filler by Weight Additive: Lubricant, UV Stabilizer and Heat Stabilizer Features: Heat Stabilized, Good UV Resistance and Lubricated Appearance: Black Information provided by TP Composites, Inc. |