Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 33% Filler by Weight Additive: Heat Stabilizer, Impact Modifier and Lubricant Features: Heat Stabilized, Impact Modified and Lubricated Appearance: Black Information provided by TP Composites, Inc. |