MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

E-Polymers EFLEX® M500 SEBS
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE; Styrene-Butadiene

Material Notes: M-series: E-FLEX M series resins are a maleic anhydride grafted (MAH) polymer concentrate designed as synthetic rubber and polyolefin manufactured by E-Polymers. It offers excellent adhesion to nylon and EVOH, as well as metal, polyolefins, cellulose, polyester, polycarbonate, glass, and foil. They are ideal for use as adhesives and tie layers in traditional food packaging applications and pipe coatings, and also in thermoplastic powder coatings, impact modification, modulus control, and glass-filled composites.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc0.910 g/ccASTM D792
Melt Flow 15 - 25 g/10 min
@Load 5.00 kg,
Temperature 230 °C
15 - 25 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
 
Descriptive Properties
MAH Graft LevelHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
API Megol AM DP2268/65PA12 SEBS Adhesion Modified Overmolding for PA
Buckeye Polymers BP FLEX A0285 BLK Thermoplastic Elastomer SEBS
Microcell Composite Company CELLOMER® S-2110 SBS Rubber Foam
Avient OnFlex™ U 5370A-E0077 Thermoplastic Elastomer (TPE)
Dynasol Calprene® H6174 Hydrogenated Rubber (SEBS)

PEPOLZ120 / 103617

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.