MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lucite International Colacryl® PD11SG Acrylic Dental Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.
Colacryl denture base resins feature fast polymerisation and a wide choice of process properties. The resins are designed to meet the requirements of BS 2487:1989/BSEN ISO 1567.

Benefits: Short cure cycles, Easy mixing, Good clarity, Excellent pigment acceptance.

Information provided by Lucite International

Key Words: Methyl Methacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 55 - 73 µm55 - 73 µm
Molecular Weight 900000 - 1.50e+6 g/mol900000 - 1.50e+6 g/mol
 
Descriptive Properties
Residual peroxide (%).27 - .39
Work Time (min)45

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucite International Colacryl® TS1326 Acrylic Dental Resin
Lucite International Colacryl® D60 Acrylic Dental Resin
Lucite International Colacryl® PD12 Acrylic Dental Resin
Lucite International Colacryl® TS 1672 Acrylic Orthodontic Polymer
Lucite International Colacryl® DP300S Acrylic Dental Resin

PLUCIT9489 / 150203

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.