MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Flexible R7542W  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.47 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 81
@Time 15.0 sec
ASTM D2240
Tensile Strength, Yield 15.2 MPaType IV, 510 mm/min; ASTM D638
Elongation at Break 300 %Type IV, 510 mm/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °CUL Temperature Rating
Brittleness Temperature -44.0 °CASTM D746
Oxygen Index 27 %
@Thickness 1.91 mm
ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 166 - 177 °C
 
Descriptive Properties
AdditiveLead Stabilizer
Agency RatingsCSA LAG (Low Acid Gas)
FeaturesFlame Retardant
FormsPellets
HCL Evolution, %12CSA C22.2 No. 0.3
Processing MethodExtrusion Coating
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Retention of Elongation, %80168 hr, UL Standard; 121°C, 1.91 mm
Retention of Tensile Strength, %100168 hr, UL Standard; 121°C, 1.91 mm
UsesCable Jacketing
 Wire & Cable Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Wire & Cable WJCK502L Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable WJKC30L PVC, Flexible
Geon® Performance Solutions Vinyl Wire & Cable WJCK504L Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable L00221 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible R7400B Polyvinyl Chloride, Flexible

PH1PN8602 / 102438

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.