MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Flexible R7400B Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 676715 sec; ASTM D2240
Tensile Strength, Yield 15.2 MPa2200 psiType IV, 510 mm/min; ASTM D638
Elongation at Break 400 %400 %Type IV, 510 mm/min; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.40e+11 ohm-cm6.40e+11 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °FUL Temperature Rating
Brittleness Temperature -50.0 °C-58.0 °FASTM D746
Oxygen Index 24 %
@Thickness 1.91 mm
24 %
@Thickness 0.0752 in
ASTM D2863
 
Processing PropertiesMetricEnglishComments
Melt Temperature 155 - 165 °C311 - 329 °F
 
Descriptive Properties
AdditiveLead Stabilizer
Agency RatingsUL QMTT2
Change in Flexural Strength100%ASTM D543; 60°C, 1.91 mm; in ASTM Oil #2, 168 hr
Change in Ultimate Elongation-19%ASTM D543; 60°C, 168 hr, in ASTM #2 Oil; 0.075 in
FeaturesFlame Retardant
 Sunlight Resistant (720 hours)
FormsPellets
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Processing MethodExtrusion Coating
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Retention of Tensile Elongation89%121°C, 1.91 mm; 500 hr, UL Standard
Retention of Tensile Strength110%121°C, 1.91 mm; 500 hr, UL Standard
UsesCable Jacketing
 Flexible Cord Jacketing
 Wire & Cable Applications
Wire TypesSJT
 SJTO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Wire & Cable WR7400L Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable WJCK504L Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable WJCK502L Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable L00221 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable WJKC30L PVC, Flexible

PH0POL0314 / 144883

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.