MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Butanediol Divinyl Ether
Categories: Fluid

Material Notes: Formula: C8H14N2

CAS: 3891-33-6

Description Butanediol divinyl ether is a colorless to yellow liquid, with a characteristic odor. It is soluble in water and with many organic solvents.

Synonyms: BDDVE, 1,4-Butandiol divinyl ether, 1,4-Divinyloxybutane Butane,1,4-bis(ethenyloxy)- Butane,1,4-bis(vinyloxy)-

Applications: Intermediate used in the production of Weathering-resistant and radiation-curing paints

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.898 g/cc
Molecular Weight 142.2 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point -8.00 °C
Flash Point 58.0 °C
Ignition Temperature 205 °C
 
Descriptive Properties
Assay>98%
Composition1,4-Butanediol<0.1%
 Vinyl-4-hydroxybutylether<2.0%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Reliance Industries PVAXX H60
BASF Elastollan® 1154 D FHF TPUR Flame Retardant Halogen Free
BASF Elastoblend LP 9192 TPUR
BASF Diethyleneglycol Divinyl Ether
BASF DEHA DI-2-Ethylhexylamine

PBASG0875 / 132508

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.