MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Elastollan® 1154 D FHF TPUR Flame Retardant Halogen Free
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.

Typical Applications: Cable sheathing, plugs and terminations, spiral tubing, films, ski boot shells, ear tags, technical moldings, e.g. mining screens, railway pads and seals.

Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°C

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³ISO 1183-1-A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5858ISO 686
Tensile Strength 20.0 MPa2900 psiafter storage in water at 80°C for 42 days; ISO 37
 30.0 MPa4350 psiISO 37
Tensile Stress at Strain  13.0 MPa
@Strain 20 %
1890 psi
@Strain 20 %
ISO 37
 19.0 MPa
@Strain 100 %
2760 psi
@Strain 100 %
ISO 37
 33.0 MPa
@Strain 300 %
4790 psi
@Strain 300 %
ISO 37
Elongation at Break 400 %400 %ISO 37
 400 %400 %after storage in water at 80°C for 42 days; ISO 37
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
DIN EN ISO 179
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
DIN EN ISO 179
Tear Strength 110 kN/m628 pliDIN ISO 34-1/Bb
Abrasion 3030[mm3; ISO 4649
Compression Set  30 %
@Temperature 23.0 °C
30 %
@Temperature 73.4 °F
ISO 815
 45 %
@Temperature 70.0 °C
45 %
@Temperature 158 °F
ISO 815
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-2V-2according to wall section
 V-0V-0
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 220 °C320 - 428 °FExtrusion
 170 - 240 °C338 - 464 °FInjection molding
Mold Temperature 20.0 - 70.0 °C68.0 - 158 °F
 
Descriptive Properties
Commercial StatusNorth America
Primary Processing TechniqueInjection molding and Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® 1185 A FHF TPUR Flame Retardant Halogen Free
BASF Elastollan® 1185 A WM TPUR
BASF Elastollan® C 85 A HPM TPUR
BASF Elastollan® 1185 A M TPUR
BASF Elastollan® C 98 A TPUR

PBASG0487 / 132120

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.