MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Cristal™ 10101 Microfiber  (discontinued **)
Categories: Polymer

Material Notes: Product Description: Cyphrex™ 10101 is a wet pulp polyester microfiber for use in wet laid nonwovens. Cyphrex™ 10101 is a less than 0.4 denier fiber with a flat or ribbon shaped cross section and a nominal width of 18 microns, a nominal thickness of 2.5 microns, and a cut length of 1.5mm. Cyphrex™ 10101 enables manufacturers to produce exceptionally uniform sheets that are lightweight and remarkably strong. The flat fibers present a novel and consistent cross section that can offer not only significant functional benefits to the nonwovens producer but also much improved processability compared with other synthetic fibers. Cyphrex™ 10101 integrates easily into existing wetlaid processes, taking media design possibilities to the next level. Unlike many other synthetic fibers, Cyphrex™ microfiber pulps are also compatible with other fiber materials such as cellulosics and glass. Cyphrex™ 10101 is another example of how Eastman is dedicated to keeping pace with your changing needs — and helping you think differently about innovative fibers for wetlaid processing.

Application/Uses:

  • Battery separators
  • Filtration
  • Membrane scrims
  • Packaging
  • Specialty nonwovens
  • Specialty papers
Key Attributes:
  • Dispersible at cellulose pulp consistencies
  • Easily dispersible synthetic microfibers
  • Enables high uniformity in nonwoven webs
  • High green strength in processing

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 1.0 %1.0 %Co-PET
 51 %51 %Polyester
 
Descriptive Properties
AppearanceWhite, pulp-like
Fiber characteristics0.4 g/9000mDenier
 1.5 mmLength
 2.5 micronsDiameter
Fiber Width18 microns

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Cellulose Acetate Propionate, Molded
Solvay GEROPON® SDS Surfactant
MOCOM (ALBIS) Cellidor® B 500-05 Cellulose Acetate Butyrate
Evonik TEGOSTAB® B 4113

PEATM5139 / 222333

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.