MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ecovio® C2224 F Blend Biodegradable Polyester
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polylactic Acid (PLA) Biopolymer

Material Notes: Ecovio® F Blend C2224 is a biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic acid (PLA, NatureWorks®). Because of the PLA content Ecovio® F Blend C2224 consists of 45% of renewable resources. Ecoflex® F Blend is the coherent phase in the structure of Ecovio® F Blend C2224 transferring the beneficial film properties of Ecoflex® F Blend into the new film product.

Application: Ecovio® F Blend C2224 has been developed for the conversion to flexible films using a blown film process. Typical applications are packaging films, hygienic films, carrier bags and compost bags. In view of numerous factors influencing functionality and shelf life of Ecovio® films and finished articles made therof the production parameters have to be tested by the converters before utilization. Additionally sufficient field tests are required to ensure the right functionality of the articles made from Ecovio® F Blend C2224.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 - 1.26 g/ccISO 1183
Water Vapor Transmission 98.0 g/m²/dayASTM F1249
Oxygen Transmission Rate 860 cc/m²/daydry; ASTM D3985
Melt Flow <= 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 2.4 - 5.2 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59ISO 868
Tensile Strength 27.0 - 35.0 MPaISO 527
Tensile Strength, Ultimate 27.0 - 35.0 MPaISO 527
Elongation at Break 250 - 320 %ISO 527
Tensile Modulus 520 - 750 MPaISO 527
Dart Drop Total Energy 380 J/cmDIN 53373
 
Thermal PropertiesOriginal ValueComments
Melting Point 110 - 120 °CDSC
 140 - 155 °CDSC
Vicat Softening Point 68.0 °CA/50; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 85 %ASTM D1003
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polylactic Acid (PLA) Biopolymer
BASF Ecovio® C2203 F Blend Biodegradable Polyester
BASF Ecovio® C2332 F Blend Biodegradable Polyester
FKuR Kunststoff Bio-Flex® F 7510 PLA Blend
Ex-Tech Plastics RenewTech™ BioPlastics Ingeo™ PLA

PBASG0008 / 131642

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.