MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Low Carbon Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Low Carbon Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.85 - 8.08 g/ccAverage value: 7.60 g/cc Grade Count:1338
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 86.0 - 550Average value: 247 Grade Count:818
Hardness, Knoop 103 - 682Average value: 278 Grade Count:728
Hardness, Rockwell B 30.0 - 105Average value: 89.4 Grade Count:764
Hardness, Rockwell C 10.0 - 64.0Average value: 31.7 Grade Count:518
Hardness, Vickers 22.0 - 661Average value: 266 Grade Count:730
Tensile Strength, Ultimate 241 - 2450 MPaAverage value: 717 MPa Grade Count:1314
Tensile Strength, Yield 140 - 2400 MPaAverage value: 521 MPa Grade Count:1306
Elongation at Break 3.00 - 48.0 %Average value: 20.1 % Grade Count:1301
Reduction of Area 13.0 - 75.0 %Average value: 53.0 % Grade Count:518
Modulus of Elasticity 183 - 213 GPaAverage value: 202 GPa Grade Count:1107
Compressive Yield Strength 152 - 1800 MPaAverage value: 1480 MPa Grade Count:14
Bulk Modulus 148 - 163 GPaAverage value: 160 GPa Grade Count:1028
Poissons Ratio 0.250 - 0.300Average value: 0.290 Grade Count:989
Fatigue Strength 170 - 772 MPaAverage value: 587 MPa Grade Count:15
Fracture Toughness 33.0 - 115 MPa-m½Average value: 68.2 MPa-m½ Grade Count:16
Machinability 50.0 - 160 %Average value: 61.3 % Grade Count:575
Shear Modulus 70.0 - 80.0 GPaAverage value: 79.6 GPa Grade Count:1111
Izod Impact 35.0 - 138 JAverage value: 96.5 J Grade Count:81
Charpy Impact 14.0 - 339 JAverage value: 54.9 J Grade Count:13
Bend Radius, Minimum 0.000 - 10.0 tAverage value: 2.46 t Grade Count:87
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000142 - 0.000142 ohm-cmAverage value: 0.0000220 ohm-cm Grade Count:959
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.1 - 16.6 µm/m-°CAverage value: 12.5 µm/m-°C Grade Count:586
Specific Heat Capacity 0.450 - 0.486 J/g-°CAverage value: 0.473 J/g-°C Grade Count:868
Thermal Conductivity 25.3 - 93.0 W/m-KAverage value: 49.5 W/m-K Grade Count:1013
Melting Point 1420 - 1460 °CAverage value: 1440 °C Grade Count:14
Maximum Service Temperature, Air 400 - 677 °CAverage value: 502 °C Grade Count:18
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.0100 - 1.50 %Average value: 0.468 % Grade Count:69
Boron, B 0.000500 - 0.00600 %Average value: 0.00268 % Grade Count:127
Carbon, C 0.00300 - 0.800 %Average value: 0.186 % Grade Count:1300
Chromium, Cr 0.200 - 10.0 %Average value: 0.879 % Grade Count:514
Cobalt, Co 7.50 - 12.0 %Average value: 8.75 % Grade Count:32
Copper, Cu 0.0200 - 1.50 %Average value: 0.371 % Grade Count:161
Iron, Fe 63.0 - 100 %Average value: 96.6 % Grade Count:1317
Lead, Pb 0.150 - 0.360 %Average value: 0.251 % Grade Count:7
Manganese, Mn 0.100 - 2.20 %Average value: 0.828 % Grade Count:1288
Molybdenum, Mo 0.0500 - 4.80 %Average value: 0.458 % Grade Count:752
Nickel, Ni 0.0300 - 18.5 %Average value: 2.59 % Grade Count:593
Niobium, Nb (Columbium, Cb) 0.00500 - 0.150 %Average value: 0.0485 % Grade Count:73
Nitrogen, N 0.00100 - 0.0700 %Average value: 0.0134 % Grade Count:38
Phosphorus, P 0.00100 - 0.400 %Average value: 0.0370 % Grade Count:1250
Silicon, Si 0.0100 - 1.00 %Average value: 0.297 % Grade Count:988
Sulfur, S 0.00100 - 0.500 %Average value: 0.0436 % Grade Count:1275
Titanium, Ti 0.0100 - 1.40 %Average value: 0.355 % Grade Count:57
Vanadium, V 0.00500 - 0.950 %Average value: 0.0912 % Grade Count:89
Zirconium, Zr 0.0100 - 0.150 %Average value: 0.0271 % Grade Count:35

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Carbon Steel
Overview of materials for Medium Carbon Steel
Overview of materials for Low Alloy Steel
Overview of materials for Stainless Steel
Overview of materials for AISI 1000 Series Steel

M01010 / 81724

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.