Description: LUPOY PC 1300-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength. Main Characteristics: High viscosity, No UV absorbers and No mold release agent Applications: Compounds, Small appliances and Packaging applications CAS: 103598-77-2 Information provided by LG Chemical |