MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUPOY GP1000L PC, Transparent
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Description: Injection Molding, PC, General Purpose, Transparency, High Flow

Application: IT/OA, E&E Housing and Components Automotive Interior

CAS: 103598-77-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Maximum Moisture Content 0.0200.020Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 22 g/10 min
@Load 1.20 kg,
Temperature 300 °C
22 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D785
Tensile Strength, Yield 61.8 MPa
@Thickness 3.20 mm
8960 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break >= 100 %
@Thickness 3.20 mm
>= 100 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength 103 MPa
@Thickness 3.20 mm
14900 psi
@Thickness 0.126 in
10mm/min; ASTM D790
Flexural Modulus 2.35 GPa
@Thickness 3.20 mm
341 ksi
@Thickness 0.126 in
10mm/min; ASTM D790
Izod Impact, Notched >= 6.86 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
>= 12.9 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cmASTM D257
Dielectric Strength 17.0 kV/mm
@Thickness 1.00 mm
432 kV/in
@Thickness 0.0394 in
ASTM D149
Arc Resistance 0.00 - 60 sec0.00 - 60 secASTM D492
Comparative Tracking Index 250 V250 VIEC 60112
Hot Wire Ignition, HWI  30 - 60 sec
@Thickness >=1.50 mm
30 - 60 sec
@Thickness >=0.0591 in
 60 - 120 sec
@Thickness >=3.00 mm
60 - 120 sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI  >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
 >= 120 arcs
@Thickness 3.00 mm
>= 120 arcs
@Thickness 0.118 in
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min0.394 - 1.00 in/min
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
@Thickness 6.40 mm
266 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 141 °C
@Load 5.00 kg
286 °F
@Load 11.0 lb
50°C/h; ASTM D1525
UL RTI, Electrical  130 °C
@Thickness >=1.50 mm
266 °F
@Thickness >=0.0591 in
 130 °C
@Thickness >=3.00 mm
266 °F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact  130 °C
@Thickness >=1.50 mm
266 °F
@Thickness >=0.0591 in
 130 °C
@Thickness >=3.00 mm
266 °F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact  130 °C
@Thickness >=1.50 mm
266 °F
@Thickness >=0.0591 in
 130 °C
@Thickness >=3.00 mm
266 °F
@Thickness >=0.118 in
Flammability, UL94  HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
 HB
@Thickness >=3.20 mm
HB
@Thickness >=0.126 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 280 °C500 - 536 °FInjection Molding
Middle Barrel Temperature 280 - 300 °C536 - 572 °FInjection Molding
Front Barrel Temperature 300 - 320 °C572 - 608 °FInjection Molding
Nozzle Temperature 300 - 320 °C572 - 608 °FInjection Molding
Melt Temperature 300 - 320 °C572 - 608 °FInjection Molding
Mold Temperature 80.0 - 120 °C176 - 248 °FInjection Molding
Drying Temperature 100 - 120 °C212 - 248 °FInjection Molding
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hourInjection Molding
Back Pressure 0.981 - 3.92 MPa142 - 569 psiInjection Molding
Screw Speed 40 - 70 rpm40 - 70 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUPOY GP1000MU PC, Transparent
LG Chemical LUPOY GP1000SW PC, Transparent
LG Chemical LUPOY GN1006FM PC, Halogen Free, Flame Retardant, Transparency
Ashley Polymers Ashlene® P1043R Polycarbonate
LG Chemical Lupoy 1300-03 Polycarbonate Resin

PLAY517 / 148527

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.