MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 2254 High Temperature Thermally Conductive Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2254 is recommended for high temperature aerospace and electronic applications where the combination of good thermal conductivity AND low electrical conductivity is required for thermal links (staking electrical components -- diodes, integrated circuits, transistors, precision resistors, or capacitors -- to chassis or circuit boards). This two-part thixotropic epoxy system is color coded for easy handling and mixing at room temperature -- although a final high temperature bake at 100°C is REQUIRED for full cure. TRA-BOND 2254 bonds strongly to ceramics (alumina, porcelain and beryllia), to glass and to many metals and plastics, and its thermal expansion coefficient is a good match for many other electronic materials (i.e. copper and aluminum) over a wide temperature range. The fully cured adhesive develops strong, durable electrically insulating/thermal conducting bonds with good impact properties, and which are also resistant to galvanic action, weathering, water, salts, mild alkalis and acids, many petroleum products, and many other organic and inorganic compounds. An additional post-cure of 4 hours at 145°C is recommended when application temperatures higher than 145°C are anticipated.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.43 g/ccMixed
Solids Content 100 %Reactive Solids Content
Viscosity 120000 cPMixed (rv #7, 10 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 97
Adhesive Bond Strength 2000 psiLap shear, alum to alum, 2 hrs @ 65°C + 2 hrs @ 100°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+15 ohm-cm
 4.00e+14 ohm-cm
@Temperature 150 °C
Dielectric Constant 6.0
@Frequency 1000 Hz
Dielectric Strength 425 V/mil
Dissipation Factor 0.010
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.0 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 1.00 W/m-K
Maximum Service Temperature, Air 205 °C
Minimum Service Temperature, Air -70.0 °C
Glass Transition Temp, Tg 130 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 hour2 hrs @ 65°C + 1 hr @ 130°C
 4.00 hour2 hrs @ 65°C + 2 hrs @ 100°C
Working Life 3.00 hour
 
Descriptive Properties
Color Light Brown
Mix Ratio, parts by weight100/5.5Resin/Hardener
Outgassing, NASA Passes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech AO 98 Aluminum Oxide Ceramic Substrate, 98% Purity
Quantum PEI - Ultem® 30% Glass Fiber Filled
Overview of materials for Medium Carbon Steel
Overview of materials for High Carbon Steel
Rogers Corporation Syron™ 7000 Thermoplastic Circuit Material

PTRAC071 / 70999

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.