MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Baytec® ENC-55P Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Baytec ENC-55P is a 450-molecular-weight polyether triol containing trimethylolpropane (TMP).

Properties / Applications: Baytec ENC-55P is a 450 molecular-weight polyether triol containing trimethylolpropane (TMP). This polyol is typically used in combination with Baytec ENC-88 isocyanate and Baylith® T or L Paste to produce solid polyurethanes with a heat deflection temperature of 70°C (158°F). Typical applications include battery sealing, cable joint sealing, and encapsulation of electrical components. As with any product, use of Baytec ENC-55P polyol in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/cc
 0.980 g/cc
@Temperature 90.0 °C
0.980 g/cc
@Temperature 194 °F
 1.01 g/cc
@Temperature 50.0 °C
1.01 g/cc
@Temperature 122 °F
Bulk Density 1.03 g/cc0.0372 lb/in³
Viscosity 520 - 700 cP520 - 700 cP
 50 cP
@Temperature 60.0 °C
50 cP
@Temperature 140 °F
 450 cP
@Temperature 30.0 °C
450 cP
@Temperature 86.0 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.25<= 0.25[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point 188 °C370 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
AppearanceClear viscous liquid
Hydroxyl number[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled
Park Aerospace Nelcote® F-562 Phenolic Prepreg, C2 Carbonized Rayon Reinforced
Park Aerospace Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced
Overview of materials for Phenolic, Novolac, Fabric Filled

PCOVEST0239 / 202022

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.