MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Description

Invision™ VX-7060UE is a developmental UV-stabilized polyolefin compound which has been formulated for soft touch, mar resistance, low gloss, excellent weatherability, and excellent low temperature toughness.
Application

Invision™ VX-6060UE is targeted for automotive extrusion appearance applications.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 6015 sec delay; ASTM D2240
Tensile Strength, Ultimate 4.10 MPaat max load; ASTM D638
Elongation at Break 500 %ASTM D638
Tensile Modulus 0.00270 GPa2% Secant, 500 mm/min; ASTM D638
 0.0147 GPa100% Secant, 500 mm/min; ASTM D638
Flexural Modulus 0.0139 GPa1.0"X3.0"X0.125", 1.3mm/min, 50 mm span; ASTM D790
 
Descriptive Properties
Colorfastness/Weatherability 1240 Delta E (kJ/m^2)SAE J1885

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polykemi AB POLYfill PP TOUCH 25325 R3 Polypropylene, Glass Fiber Reinforced, Scratch Resistant
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic
A. Schulman INVISION™ VX-5065UI Soft Touch Polyolefin Thermoplastic
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer

PASHU059 / 25023

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.