MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polykemi AB POLYfill PP TOUCH 25325 R3 Polypropylene, Glass Fiber Reinforced, Scratch Resistant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes:

Information provided by Polykemi AB

Key Words: Polypropylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Filler Content 25 %25 %±2%; Polykemi
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/inISO 2577
Melt Index of Compound 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 53
@Time 15.0 sec
53
@Time 0.00417 hour
ASTM D2240
Flexural Strength <= 43.0 MPa<= 6240 psiISO 178
Flexural Modulus 2.30 GPa
@Temperature 23.0 °C
334 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched  2.50 J/cm²
@Temperature -20.0 °C
11.9 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 3.10 J/cm²
@Temperature 23.0 °C
14.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °F120°C/h; ISO 75/1
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Glow Wire Test 750 °C
@Thickness 2.00 mm
1380 °F
@Thickness 0.0787 in
IEC 695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 205 - 260 °C401 - 500 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 2 - 4 hour2 - 4 hourin circulation dryer
 2 - 4 hour2 - 4 hourin desiccant air dryer
Injection Pressure 40.0 - 110 MPa5800 - 16000 psi
Back Pressure 1.00 - 2.00 MPa145 - 290 psi
 
Descriptive Properties
Holding Pressure20-40% of injection pressure
Injection SpeedHigh
Scratch Resistance, 10N (dL)< 0.210N Fine Structure; ISO 1518/D65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polykemi AB POLYfill PP TOUCH 34725 Polypropylene, Glass Fiber Reinforced
Polykemi AB POLYfill PP TOUCH 25325 Polypropylene, Glass Fiber Reinforced
A. Schulman INVISION™ VX-7060UE Soft Touch Polyolefin Thermoplastic
A. Schulman INVISION™ VX-5070UI Soft Touch Polyolefin Thermoplastic
A. Schulman INVISION™ VX-5065UI Soft Touch Polyolefin Thermoplastic

PPOLYK279 / 123004

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.