MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® 5628 LDPE Blown Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: This low density polyethylene is tailored for blown film applications that require:
  • Superior strength
  • Good abrasion and tear resistance
  • Exceptional shrink and shrink tension
  • High coefficient of friction
Typical blown film applications include:
  • Heavy duty packaging
  • Pallet shrink
  • Case shrink wrap
  • C&A film and container liners

Information provided by Chevron Phillips.

Formerly branded with the MarFlex® trade name.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.922 g/ccASTM D1505
Water Vapor Transmission 10.85 g/m²/dayASTM F1249
Oxygen Transmission Rate 4000 cc/m²/dayASTM D3985
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 1500 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 225 %ASTM D882
Film Elongation at Break, TD 550 %ASTM D882
Coefficient of Friction 0.50ASTM D1894
Elmendorf Tear Strength MD 230 gASTM D1922
Elmendorf Tear Strength TD 250 gASTM D882
Dart Drop Test 200 gASTM D1709
Film Tensile Strength at Break, MD 29.0 MPaASTM D882
Film Tensile Strength at Break, TD 27.0 MPaASTM D882
1% Secant Modulus, MD 26000 psiASTM D882
1% Secant Modulus, TD 30000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 98.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 7.0 %ASTM D1003
Gloss 100 %60°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 111 °CASTM D3418
 
Descriptive Properties
AntiblockLow

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Purell PE 1810E Low Density Polyethylene (LDPE)
Versalis Riblene® BD 30 Low Density Polyethylene - Blow Molding
Braskem F0421D Blown Film Extrusion Low Density Polyethylene
Sibur 15303-003 Low Density Polyethylene
Eastman D4032-F Polyethylene

PCHEVD000 / 20626

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.