MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polystyrene, Flame Retardant
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.950 - 1.20 g/ccAverage value: 1.13 g/cc Grade Count:118
Water Absorption 0.000 - 0.300 %Average value: 0.0824 % Grade Count:37
Moisture Absorption at Equilibrium 0.0400 - 0.300 %Average value: 0.123 % Grade Count:6
Particle Size 90.0 - 1600 µmAverage value: 1070 µm Grade Count:4
Maximum Moisture Content 0.0100Average value: 0.0100 Grade Count:5
 0.200 - 0.200
@Temperature 120 - 120 °C
Average value: 0.200 Grade Count:2
 0.200 - 0.200
@Time 299 - 299 sec
Average value: 0.200 Grade Count:2
Linear Mold Shrinkage 0.00200 - 0.00800 cm/cmAverage value: 0.00512 cm/cm Grade Count:89
Linear Mold Shrinkage, Transverse 0.00200 - 0.00600 cm/cmAverage value: 0.00350 cm/cm Grade Count:3
Melt Flow 2.50 - 25.0 g/10 minAverage value: 9.61 g/10 min Grade Count:112
Spiral Flow 34.0 - 56.0 cm
@Temperature 220 - 260 °C
Average value: 45.8 cm Grade Count:5
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 45.0 - 94.0Average value: 61.1 Grade Count:8
Hardness, Rockwell M 55.0 - 65.0Average value: 59.2 Grade Count:6
Hardness, Rockwell R 83.0 - 110Average value: 94.7 Grade Count:18
Tensile Strength, Ultimate 12.4 - 48.3 MPaAverage value: 26.1 MPa Grade Count:63
Tensile Strength, Yield 14.0 - 55.0 MPaAverage value: 26.6 MPa Grade Count:79
Elongation at Break 1.00 - 80.0 %Average value: 40.7 % Grade Count:109
Elongation at Yield 1.00 - 5.00 %Average value: 2.69 % Grade Count:16
Modulus of Elasticity 1.38 - 3.45 GPaAverage value: 2.12 GPa Grade Count:31
Flexural Yield Strength 25.5 - 82.7 MPaAverage value: 39.9 MPa Grade Count:72
Flexural Modulus 1.40 - 17.7 GPaAverage value: 2.28 GPa Grade Count:103
Izod Impact, Notched 0.107 - 1.71 J/cmAverage value: 1.01 J/cm Grade Count:81
 0.600 - 0.800 J/cm
@Temperature 0.000 - 0.000 °C
Average value: 0.468 J/cm Grade Count:4
 0.392266 - 0.490332 J/cm
@Temperature -30.0 - -30.0 °C
Average value: 0.468 J/cm Grade Count:5
 0.392266 - 0.490332 J/cm
@Thickness 3.20 - 6.40 mm
Average value: 0.468 J/cm Grade Count:5
Izod Impact, Notched (ISO) 5.00 - 11.0 kJ/m²Average value: 7.04 kJ/m² Grade Count:24
Charpy Impact Unnotched 2.00 - 10.0 J/cm²Average value: 6.11 J/cm² Grade Count:13
 4.00 - 8.00 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 5.71 J/cm² Grade Count:7
Charpy Impact, Notched 0.200 - 1.20 J/cm²Average value: 0.682 J/cm² Grade Count:16
Tensile Creep Modulus, 1 hour 1600 - 2200 MPaAverage value: 1930 MPa Grade Count:3
Tensile Creep Modulus, 1000 hours 1200 - 1600 MPaAverage value: 1400 MPa Grade Count:4
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+12 - 1.00e+16 ohm-cmAverage value: 7.90e+15 ohm-cm Grade Count:39
Surface Resistance 1.00e+12 - 1.00e+15 ohmAverage value: 1.04e+14 ohm Grade Count:22
Dielectric Constant 2.00 - 3.00Average value: 2.42 Grade Count:17
Dielectric Strength 17.7 - 160 kV/mmAverage value: 69.6 kV/mm Grade Count:15
Dissipation Factor 0.000400 - 0.00500Average value: 0.00110 Grade Count:15
Arc Resistance 60.0 - 180 secAverage value: 120 sec Grade Count:5
Comparative Tracking Index 225 - 600 VAverage value: 363 V Grade Count:18
Hot Wire Ignition, HWI 7.00 - 30.0 secAverage value: 21.1 sec Grade Count:5
High Amp Arc Ignition, HAI 60.0 - 120 arcsAverage value: 116 arcs Grade Count:5
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/minAverage value: 17.7 mm/min Grade Count:5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 - 100 µm/m-°CAverage value: 80.4 µm/m-°C Grade Count:14
Hot Ball Pressure Test 75.0 - 85.0 °CAverage value: 80.3 °C Grade Count:13
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 96.1 °CAverage value: 84.6 °C Grade Count:20
Deflection Temperature at 1.8 MPa (264 psi) 60.0 - 91.0 °CAverage value: 79.0 °C Grade Count:80
Vicat Softening Point 80.0 - 219 °CAverage value: 94.2 °C Grade Count:93
Heat Distortion Temperature 78.9 - 94.0 °CAverage value: 84.2 °C Grade Count:6
UL RTI, Electrical 50.0 °CAverage value: 50.0 °C Grade Count:5
UL RTI, Mechanical with Impact 50.0 °CAverage value: 50.0 °C Grade Count:5
UL RTI, Mechanical without Impact 50.0 °CAverage value: 50.0 °C Grade Count:5
Flammability, UL94 V-2 - 5VAGrade Count:110
Oxygen Index 26.0 %Average value: 26.0 % Grade Count:6
Glow Wire Test 650 - 960 °CAverage value: 879 °C Grade Count:21
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 250 °CAverage value: 243 °C Grade Count:23
Nozzle Temperature 200 - 232 °CAverage value: 213 °C Grade Count:9
Melt Temperature 160 - 300 °CAverage value: 217 °C Grade Count:61
Mold Temperature 10.0 - 80.0 °CAverage value: 46.2 °C Grade Count:53
Drying Temperature 60.0 - 90.0 °CAverage value: 70.6 °C Grade Count:49
Injection Pressure 60.0 - 103 MPaAverage value: 82.1 MPa Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polystyrene, Molded, Unreinforced
Overview of materials for Polystyrene, Heat Resistant Grade
Overview of materials for Polystyrene, Extrusion Grade
Overview of materials for Polystyrene, Impact Modified
Overview of materials for Polystyrene, Glass Filled

O4809 / 78416

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.