MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes:
  • Industrial pallet wrap stretch film applications
  • Premium film packaging applications
  • Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a

TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed for cast stretch film applications such as industrial pallet wrap. Films containing HS-7021 offer outstanding extensibility and cling properties.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccASTM D792
Thickness 0.800 mil
Melt Flow 3.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1779 psiASTM D882
Film Tensile Strength at Yield, TD 1620 psiASTM D882
Film Elongation at Break, MD 584 %ASTM D882
Film Elongation at Break, TD 875 %ASTM D882
Elongation, Ultimate 363 %on-pallet testing; Highlight Industries Method
Secant Modulus, MD 0.1491 GPa2% Secant; ASTM D882
Secant Modulus, TD 0.1584 GPa2% Secant; ASTM D882
Impact 8.0[lbf]; Puncture Resistance Force; Dow Method
 272[ft-lbf/in3]; Puncture Resistance; Dow Method
Puncture Energy 28.0 in-lbDow Method
Elmendorf Tear Strength MD 164 gMethod B; ASTM D1922
Elmendorf Tear Strength TD 567 gMethod B; ASTM D1922
Elmendorf Tear Strength, MD 205 g/milASTM D1922
Elmendorf Tear Strength, TD 708.75 g/milASTM D1922
Dart Drop Test 96.0 gMethod A; ASTM D1709
 <= 100 gMethod B; ASTM D1709
Film Tensile Strength at Break, MD 8727 psiASTM D882
Film Tensile Strength at Break, TD 5913 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 123 °CDow Method (DSC)
Vicat Softening Point 100 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 1.0 %ASTM D1003
Gloss 95 %45°; ASTM D2457
 157 %20°; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Cling g208ASTM D5458, unstretched

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow ELITE™ 5100G Enhanced Polyethylene Resin
Dow DOWLEX™ 2070G Linear Low Density Polyethylene
Dow DOWLEX™ 2078G Linear Low Density Polyethylene
Dow Bynel® 4140 Anhydride Modified LLDPE
Dow DOWLEX™ 2038.68G Linear Low Density Polyethylene

PDOW1438 / 30656

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.