MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Maxxam™ PPH-40G Nat PP Homopolymer with 40% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes: Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium carbonate, glass and talc to provide a desired balance of properties including stiffness, durability, impact resistance and heat resistance. Custom grades are available with features such as UV stabilizers, heat stabilizers, custom color, high impact, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
Filler Content 40 %40 %
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9999ASTM D785
Tensile Strength, Yield 70.3 MPa10200 psiType I, 51 mm/min; ASTM D638
Elongation at Break 5.0 %5.0 %Type I, 51 mm/min; ASTM D638
Flexural Strength 100 MPa14500 psiASTM D790
Flexural Modulus 6.55 GPa950 ksiASTM D790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
1.00 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Izod Impact, Unnotched 1.49 J/cm
@Thickness 3.18 mm
2.79 ft-lb/in
@Thickness 0.125 in
Injection Molded; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 162 °C
@Thickness 3.18 mm
324 °F
@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
All colors; UL 94
 
Descriptive Properties
AppearanceNatural Color
FeaturesGeneral Purpose
 Homopolymer
FormsPellets
Generic NamePolypropylene Homopolymer
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Maxxam™ PPC-40G Nat PP Copolymer with 40% Glass Fiber
Avient Maxxam™ PD 40 TF Black Polypropylene Homopolymer (PP Homopolymer)
A. Schulman TPP40AJ38BK 40% Talc Filled, Heat-Stabilized, Controlled Rheology, Homopolymer Polypropylene containing 25% P.C.R.
Avient Maxxam™ PPC-40T Black PP Copolymer with 40% Talc
Inno-Comp INNOPOL® CS 1-6140 N 40% Talc-Filled Polypropylene Homopolymer

PH1PN9216 / 103052

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.