MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman TPP40AJ38BK 40% Talc Filled, Heat-Stabilized, Controlled Rheology, Homopolymer Polypropylene containing 25% P.C.R.
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Talc Filler

Material Notes: 40% Talc Filled, Heat-Stabilized, Controlled Rheology, Homopolymer Polypropylene containing 25% P.C.R.

Description: Color match black

Applications: Primary end use is for instrument cluster masks.

Specifications: Meets/exceeds Ford Engineering Material Specification WSK-M4D644-A3

Comments:
Tensile/Izod Change (1000 hrs./140°C): +5/+10%; WSK-M4D644A3 Specification: ±15/±15; ISO 188
Mineral Content: 38 %;WSK-M4D644-A3 Specification: 35.0-40.0; ISO 3451/1A
Material Pre-dry: Normally it is not necessary to pre-dry this material. However, if conditions dictate drying to optimize material properties and part appearance then dry in a desiccant dryer at 180°F for 2-3 hours or 160°F for >4 hours.
Manifolds: Maintain manifolds, runners and tips 10 to 20°F above the front one temperature to allow easier filling. (Gate drool is best eliminated using screw decompression rather than reducing tip temperature.)
Back Pressure (Range): 20-50 psi. Injection Speed: medium to fast. Screw Speed: medium. Injection Pressure: Adjust to just above a short shot. Injection Time: Adjust to just above a short shot. Cushion (Range): 0.2-0.5 in. Nozzle Type: Free flowing/Standard.
Some conditions may have to be altered to obtain acceptable parts. Please do not run too cold, molded in stress and rough surface may become a problem. If you must run below melt or temperatures recommended for dimensional precision you may compromise impact and esthetics. Retest parts to confirm performance.

Data provided by Ferro Corporation - Specialty Plastics Group.

A. Schulman has acquired the Ferro specialty plastics business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³WSK-M4D644-A3 Specification: 1.19-1.25 g/cc; ISO R 527
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inISO 2577
Melt Flow 13.8 g/10 min13.8 g/10 minWSK-M4D644-A3 Specification: 12.0-18.0 g/10 min; ISO R 527
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 27.4 MPa3970 psiWSK-M4D644-A3 Specification: 24 MPa Min.; ISO R 527
Flexural Modulus 3.80 GPa551 ksiWSK-M4D644-A3 Specification: 3.6 GPa Min.; ISO R 527
Izod Impact, Notched (ISO) 2.30 kJ/m²1.09 ft-lb/in²WSK-M4D644-A3 Specification: 2 kJ/m² Min.; ISO R 527
 1.70 kJ/m²
@Temperature -40.0 °C
0.809 ft-lb/in²
@Temperature -40.0 °F
WSK-M4D644-A3 Specification: 1.4 kJ/m² Min.; ISO R 527
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FWSK-M4D644-A3 Specification: 118°C; ISO R 527
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °FWSK-M4D644-A3 Specification: 67°C; ISO R 527
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 204 - 218 °C400 - 425 °F
Middle Barrel Temperature 210 - 218 °C410 - 425 °F
Front Barrel Temperature 213 - 224 °C415 - 435 °F
Nozzle Temperature 216 - 227 °C420 - 440 °F
Mold Temperature 37.8 - 48.9 °C100 - 120 °FCore. Cooler temperatures may be needed to maintain dimensions or eliminate sinks in thick sections.
 43.3 - 54.4 °C110 - 130 °FCavity
Drying Temperature 82.2 °C180 °F2-3 hrs at 180°F or 4+ hours at 160°F.
Dry Time 2 - 3 hour2 - 3 hour
 
Descriptive Properties
ColorColor match black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Maxxam™ PPC-40G Nat PP Copolymer with 40% Glass Fiber
Avient Maxxam™ PPH-40G Nat PP Homopolymer with 40% Glass Fiber
A. Schulman TPP40AC27NA 40% Talc Filled, Heat Stabilized, Homopolymer Polypropylene
A. Schulman Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled
A. Schulman TPP40AC38WH 40% Talc and Titanium Dioxide Filled, Heat-Stabilized, Homopolymer Polypropylene

PFERRO69 / 38183

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.