MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik Kanthal® APMT™
Categories: Other Engineering Material

Material Notes: Tubes in Kanthal APMT are seamless and produced by extrusion. They are suitable for use in a wide range of temperatures and atmospheres, covering many applications and processes in various industries.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.20 g/cc0.260 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  2.00 MPa
@Temperature 1150 °C
290 psi
@Temperature 2100 °F
 10.0 MPa
@Temperature 950 °C
1450 psi
@Temperature 1740 °F
 22.0 MPa
@Temperature 800 °C
3190 psi
@Temperature 1470 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.0 µm/m-°C
@Temperature 20.0 - 250 °C
6.67 µin/in-°F
@Temperature 68.0 - 482 °F
 13.0 µm/m-°C
@Temperature 20.0 - 500 °C
7.22 µin/in-°F
@Temperature 68.0 - 932 °F
 14.0 µm/m-°C
@Temperature 20.0 - 750 °C
7.78 µin/in-°F
@Temperature 68.0 - 1380 °F
 15.0 µm/m-°C
@Temperature 20.0 - 1000 °C
8.33 µin/in-°F
@Temperature 68.0 - 1830 °F
 15.0 µm/m-°C
@Temperature 20.0 - 1250 °C
8.33 µin/in-°F
@Temperature 68.0 - 2280 °F
Specific Heat Capacity  >= 0.480 J/g-°C
@Temperature 20.0 °C
>= 0.115 BTU/lb-°F
@Temperature 68.0 °F
 >= 0.560 J/g-°C
@Temperature 200 °C
>= 0.134 BTU/lb-°F
@Temperature 392 °F
 >= 0.640 J/g-°C
@Temperature 400 °C
>= 0.153 BTU/lb-°F
@Temperature 752 °F
 >= 0.670 J/g-°C
@Temperature 800 °C
>= 0.160 BTU/lb-°F
@Temperature 1470 °F
 >= 0.690 J/g-°C
@Temperature 1000 °C
>= 0.165 BTU/lb-°F
@Temperature 1830 °F
 >= 0.700 J/g-°C
@Temperature 1200 °C
>= 0.167 BTU/lb-°F
@Temperature 2190 °F
 >= 0.710 J/g-°C
@Temperature 600 °C
>= 0.170 BTU/lb-°F
@Temperature 1110 °F
 >= 0.740 J/g-°C
@Temperature 1400 °C
>= 0.177 BTU/lb-°F
@Temperature 2550 °F
Thermal Conductivity  11.0 W/m-K
@Temperature 50.0 °C
76.3 BTU-in/hr-ft²-°F
@Temperature 122 °F
 21.0 W/m-K
@Temperature 600 °C
146 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 23.0 W/m-K
@Temperature 800 °C
160 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 27.0 W/m-K
@Temperature 1000 °C
187 BTU-in/hr-ft²-°F
@Temperature 1830 °F
 29.0 W/m-K
@Temperature 1200 °C
201 BTU-in/hr-ft²-°F
@Temperature 2190 °F
 32.0 W/m-K
@Temperature 1400 °C
222 BTU-in/hr-ft²-°F
@Temperature 2550 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.0 %5.0 %
Carbon, C <= 0.050 %<= 0.050 %
Chromium, Cr 22 %22 %
Iron, Fe >= 68.85 %>= 68.85 %As Balance
Manganese, Mn <= 0.40 %<= 0.40 %
Molybdenum, Mo 3.0 %3.0 %
Silicon, Si <= 0.70 %<= 0.70 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik Kanthal APMT Seamless tube and pipe
AISI Type 304HN Stainless Steel
AISI 304H Stainless Steel, Austenitic
304 Stainless Steel

NSANDV5276 / 199840

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.