MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI 304H Stainless Steel, Austenitic
Categories: Metal; Ferrous Metal; Stainless Steel; Cast Stainless Steel; T 300 Series Stainless Steel

Material Notes: 18Cr-8Ni STAINLESS STEEL FOR BOILER AND HEAT EXCHANGER SEAMLESS TUBES (SUS 304H TB)

Creep and rupture data provided by NIMS

Key Words: JIS G3463(94) SUS 304-H TB; UNS S30409
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B <= 90<= 90
Tensile Strength, Ultimate 520 MPa75400 psi
Tensile Strength, Yield 205 MPa29700 psi
Rupture Strength  22.0 - 51.0 MPa
@Temperature 700 °C,
Time 3.60e+8 sec
3190 - 7400 psi
@Temperature 1290 °F,
Time 100000 hour
 32.0 - 61.0 MPa
@Temperature 675 °C,
Time 3.60e+8 sec
4640 - 8850 psi
@Temperature 1250 °F,
Time 100000 hour
 49.0 - 77.0 MPa
@Temperature 650 °C,
Time 3.60e+8 sec
7110 - 11200 psi
@Temperature 1200 °F,
Time 100000 hour
 74.0 - 107 MPa
@Temperature 625 °C,
Time 3.60e+8 sec
10700 - 15500 psi
@Temperature 1160 °F,
Time 100000 hour
 99.0 - 143 MPa
@Temperature 600 °C,
Time 3.60e+8 sec
14400 - 20700 psi
@Temperature 1110 °F,
Time 100000 hour
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.040 - 0.10 %0.040 - 0.10 %
Chromium, Cr 18 - 20 %18 - 20 %
Iron, Fe 66.08 - 73.96 %66.08 - 73.96 %
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 8.0 - 11 %8.0 - 11 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 0.75 %<= 0.75 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
304 Stainless Steel
AISI Type 316L Stainless Steel, annealed bar
AISI Type 304L Stainless Steel
AISI Type 304HN Stainless Steel
Outokumpu 253MA® High Temperature Austenitic Stainless Steel

NIMS020 / 77537

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.