MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 304H Stainless Steel, Austenitic
Categories: Metal; Ferrous Metal; Stainless Steel; Cast Stainless Steel; T 300 Series Stainless Steel

Material Notes: 18Cr-8Ni STAINLESS STEEL FOR BOILER AND HEAT EXCHANGER SEAMLESS TUBES (SUS 304H TB)

Creep and rupture data provided by NIMS

Key Words: JIS G3463(94) SUS 304-H TB; UNS S30409
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B <= 90
Tensile Strength, Ultimate 520 MPa
Tensile Strength, Yield 205 MPa
Rupture Strength 22.0 - 51.0 MPa
@Temperature 700 °C,
Time 3.60e+8 sec
 32.0 - 61.0 MPa
@Temperature 675 °C,
Time 3.60e+8 sec
 49.0 - 77.0 MPa
@Temperature 650 °C,
Time 3.60e+8 sec
 74.0 - 107 MPa
@Temperature 625 °C,
Time 3.60e+8 sec
 99.0 - 143 MPa
@Temperature 600 °C,
Time 3.60e+8 sec
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.040 - 0.10 %
Chromium, Cr 18 - 20 %
Iron, Fe 66.08 - 73.96 %
Manganese, Mn <= 2.0 %
Nickel, Ni 8.0 - 11 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 0.75 %
Sulfur, S <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
304 Stainless Steel
AISI Type 316L Stainless Steel, annealed bar
AISI Type 304L Stainless Steel
AISI Type 304HN Stainless Steel
Outokumpu 253MA® High Temperature Austenitic Stainless Steel

NIMS020 / 77537

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.